Aluminum 7050A Composition Spec
Subcategory: 7000 Series Aluminum Alloy; Aluminum Alloy; Metal; Nonferrous Metal
Close Analogs: Composition Notes: Aluminum content reported is calculated as remainder. Composition information provided by the Aluminum Association and is not for design.
Key Words: Aluminium 7050A; AA7050A
| Component | Wt. % |  | | | Al | 87.3 - 90.9 | | | Cr | Max 0.04 | | | Cu | 1.7 - 2.4 | | | Fe | Max 0.15 | | | Mg | 1.7 - 2.6 | |
| | Component | Wt. % |  | | | Mn | Max 0.04 | | | Ni | Max 0.03 | | | Other, each | Max 0.05 | | | Other, total | Max 0.15 | |
| | Component | Wt. % |  | | | Si | Max 0.12 | | | Ti | Max 0.06 | | | Zn | 5.7 - 6.9 | | | Zr | 0.05 - 0.12 | |
|
Material Notes: This data sheet has only a limited amount of property data. Most MatWeb aluminum entries, especially entries with a specific temper in the name, have much more property data. Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.
| Physical Properties | Metric | English | Comments |
|
| Density | 2.82 g/cc | 0.102 lb/in³ | AA; Typical |
Processing Properties |
|
| Annealing Temperature | 413 °C | 775 °F | |
| Solution Temperature | 477 °C | 890 °F | |
| Aging Temperature | 121 - 177 °C | 250 - 350 °F | |
References for this datasheet.
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. MatWeb data and tools provided by MatWeb, LLC.
|