300M Ultrahigh Strength Steel
Subcategory: Carbon Steel; Ferrous Metal; Low Alloy Steel; Medium Carbon Steel; Metal
| Component | Wt. % |  | | | C | 0.4 - 0.46 | | | Cr | 0.7 - 0.95 | | | Fe | 93.4 - 94.8 | | | Mn | 0.65 - 0.9 | |
| | Component | Wt. % |  | | | Mo | 0.3 - 0.45 | | | Ni | 1.65 - 2 | | | P | Max 0.035 | |
| | Component | Wt. % |  | | | S | Max 0.04 | | | Si | 1.45 - 1.8 | | | V | Min 0.05 | |
|
Material Notes: Iron content calculated as balance. Phosphorous and sulfur content may vary. Silicon content helps to prevent embrittlement when tempered at low temperatures. Easily processed by hot forging; slow cooling is needed to prevent stress cracking.
| Physical Properties | Metric | English | Comments |
|
| Density | 7.87 g/cc | 0.284 lb/in³ | Typical of steel |
Mechanical Properties |
|
| Modulus of Elasticity | 205 GPa | 29700 ksi | Typical of steel |
| Poisson's Ratio | 0.28 | 0.28 | Calculated |
| Shear Modulus | 80 GPa | 11600 ksi | Typical of steel |
References for this datasheet.
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. MatWeb data and tools provided by MatWeb, LLC.
|