VascoMax® C-350 Specialty Steel, Heat Treatment: 927°C (1700°F) + Age
Subcategory: Ferrous Metal; Maraging Steel; Metal
Key Words: Allvac, an Allegheny Teledyne Company; Maraging Steel, PWA 1091. PDS 10705Z2.
Component | Wt. % | | | Al | 0.1 | | C | 0.02 | | Co | 12 | | Fe | 63 | |
| Component | Wt. % | | | Mn | 0.05 | | Mo | 4.8 | | Ni | 18.5 | | P | 0.005 | |
| Component | Wt. % | | | S | 0.005 | | Si | 0.05 | | Ti | 1.4 | |
|
Material Notes: Iron content calculated as remainder. Data provided by Allvac. Applications: Missile components. Tooling. Spring wire for valve springs in high-performance internal combustion engines.
Physical Properties | Metric | English | Comments |
|
Density | 8.08 g/cc | 0.292 lb/in³ | |
Mechanical Properties |
|
Hardness, Brinell | 529 | 529 | Estimated from Rockwell C value for Brinell test with 3000 kg load/10 mm diameter ball |
Hardness, Knoop | 585 | 585 | Estimated from Rockwell C value. |
Hardness, Rockwell C | 53 | 53 | |
Hardness, Vickers | 559 | 559 | Estimated from Rockwell C value. |
Tensile Strength, Ultimate | 2310 MPa | 335000 psi | |
Tensile Strength, Yield | 2242 MPa | 325000 psi | 0.2% Offset |
Elongation at Break | 6 % | 6 % | |
Reduction of Area | 25 % | 25 % | |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. MatWeb data and tools provided by MatWeb, LLC.
|