Vasco® Greek Ascoloy Specialty Steel, Heat Treatment: 871°C (1600°F) + Age
Subcategory: Ferrous Metal; Metal; Stainless Steel; T 400 Series Stainless Steel
Key Words: Allvac, an Allegheny Teledyne Company, UNS S41800; AMS 5508, 5616. MTS 1150
| Component | Wt. % |  | | | C | 0.18 | | | Cr | 13 | | | Fe | 81 | |
| | Component | Wt. % |  | | | Mn | 0.25 | | | Ni | 2 | | | P | 0.02 | |
| | Component | Wt. % |  | | | S | 0.015 | | | Si | 0.25 | | | W | 3 | |
|
Material Notes: Iron content calculated as remainder. Data provided by Allvac. Applications: Compressor blades, vanes, disks, shafts, wheels, fasteners, gas turbine and jet engine components.
| Physical Properties | Metric | English | Comments |
|
| Density | 7.86 g/cc | 0.284 lb/in³ | |
Mechanical Properties |
|
| Hardness, Rockwell B | 130 | 130 | As reported by the manufacturer. Beyond normal Rockwell B hardness range. |
| Tensile Strength, Ultimate | 1172 MPa | 170000 psi | |
| Tensile Strength, Yield | 1034 MPa | 150000 psi | 0.2% Offset |
| Elongation at Break | 10 % | 10 % | |
| Reduction of Area | 32 % | 32 % | |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. MatWeb data and tools provided by MatWeb, LLC.
|