Vasco® Jethete® M152 Specialty Steel, Heat Treatment: 691°C (1275°F) Anneal
Subcategory: Ferrous Metal; Metal; Stainless Steel
Key Words: Allvac, an Allegheny Teledyne Company, UNS S64152; AMS 5719
| Component | Wt. % |  | | | C | 0.12 | | | Cr | 16.8 | | | Fe | 78 | | | Mn | 0.7 | |
| | Component | Wt. % |  | | | Mo | 1.8 | | | N | 0.03 | | | Ni | 2.5 | | | P | 0.013 | |
| | Component | Wt. % |  | | | S | 0.013 | | | Si | 0.18 | | | V | 0.33 | |
|
Material Notes: Iron content calculated as remainder. Data provided by Allvac. Applications: Rings and structural components for land-based turbines.
| Physical Properties | Metric | English | Comments |
|
| Density | 7.75 g/cc | 0.28 lb/in³ | |
Mechanical Properties |
|
| Hardness, Brinell | 326 | 326 | Estimated from Rockwell C value for Brinell test with 3000 kg load/10 mm diameter ball |
| Hardness, Knoop | 354 | 354 | Estimated from Rockwell C value. |
| Hardness, Rockwell C | 35 | 35 | |
| Hardness, Vickers | 341 | 341 | Estimated from Rockwell C value. |
| Tensile Strength, Ultimate | 1104 MPa | 160000 psi | |
| Tensile Strength, Yield | 966 MPa | 140000 psi | 0.2% Offset |
| Elongation at Break | 20 % | 20 % | |
| Reduction of Area | 70 % | 70 % | |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. MatWeb data and tools provided by MatWeb, LLC.
|