Special Metals INCO® A-286 Iron-Nickel-Chromium Alloy
Subcategory: Iron Base; Metal; Superalloy
| Component | Wt. % |  | | | Al | Max 0.35 | | | B | 0.001 - 0.01 | | | C | Max 0.08 | | | Cr | 13.5 - 16 | |
| | Component | Wt. % |  | | | Fe | 60 | | | Mn | Max 2 | | | Mo | 1 - 1.5 | | | Ni | 24 - 27 | |
| | Component | Wt. % |  | | | S | Max 0.03 | | | Ti | 1.9 - 2.35 | | | V | 0.1 - 0.5 | | | W | 3 - 4.5 | |
|
Material Notes: Iron content calculated as remainder. Data provided by the manufacturer, Special Metals.
| Physical Properties | Metric | English | Comments |
|
| Density | 7.94 g/cc | 0.287 lb/in³ | |
Mechanical Properties |
|
| Modulus of Elasticity | 201 GPa | 29200 ksi | |
Electrical Properties |
|
| Electrical Resistivity | 9.1e-005 ohm-cm | 9.1e-005 ohm-cm | |
| Magnetic Permeability | 1.007 | 1.007 | at 200 Oersted (15.9 kA/m) |
Thermal Properties |
|
| CTE, linear 20°C | 16.4 µm/m-°C | 9.11 µin/in-°F | Mean 27-100°C |
| CTE, linear 250°C | 16.9 µm/m-°C | 9.39 µin/in-°F | Mean 27-300°C |
| CTE, linear 500°C | 17.5 µm/m-°C | 9.72 µin/in-°F | Mean 27-500°C |
| CTE, linear 1000°C | 17.7 µm/m-°C | 9.83 µin/in-°F | Mean 27-700°C |
| Specific Heat Capacity | 0.419 J/g-°C | 0.1 BTU/lb-°F | |
| Thermal Conductivity | 12.7 W/m-K | 88.1 BTU-in/hr-ft²-°F | |
| Melting Point | 1370 - 1430 °C | 2500 - 2610 °F | |
| Solidus | 1370 °C | 2500 °F | |
| Liquidus | 1430 °C | 2610 °F | |
| Maximum Service Temperature, Air | 700 °C | 1290 °F | good strength and oxidation resistance |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. MatWeb data and tools provided by MatWeb, LLC.
|