Allegheny Ludlum AM 355™ High Strength Alloy, UNS S35500
 Subcategory: Ferrous Metal; Metal; T 300 Series Stainless Steel 
| Component |    Wt. % |   |   |  | Cr | 15.5 |   |  | Fe | 76.5 |   |  | Mn | 0.95 |   |  | Mo | 2.75 |   |  | Ni | 4.3 |   |  
  |   
Material Notes:  Iron content above calculated as remainder. Available in sheet and strip.  For use in high-strength aerospace applications. Information provided by Allegheny Ludlum 
We're sorry, but our sources do not report any other information for this material. Sometimes you will see this message during a MatWeb internal update, especially around 07:00 GMT. 
	 Some of the values displayed above may have been converted from their original units and/or rounded in 
	order to display the information in a consistant format.  Users requiring more precise data for scientific or 
	engineering calculations can click on the property value to see the original value as well as raw conversions 
	to equivalent units.  We advise that you only use the original value or one of its raw conversions in your 
	calculations to minimize rounding error.  We also ask that you refer to MatWeb's disclaimer and terms of use 
	regarding this information.  MatWeb data and tools provided by MatWeb, LLC. 
				 |