Allegheny Ludlum Grade 3 Titanium (UNS R50550)
Subcategory: Metal; Nonferrous Metal; Titanium Alloy; Unalloyed/Modified Titanium
Key Words: ASTM B-265; ASME SB-265; AMS 4900; DIN 3.7055
| Component | Wt. % |  | | | C | Max 0.1 | | | Fe | Max 0.3 | | | H | Max 0.015 | | | N | Max 0.05 | | | O | Max 0.35 | | | Ti | Min 99.2 | |
|
Material Notes: Titanium content above calculated as remainder. Uses: CPI equipment, industrial components, heat exchangers. Mechanical property data below is typical of annealed samples at room temperature. Information provided by Allegheny Ludlum.
| Physical Properties | Metric | English | Comments |
|
| Density | 4.52 g/cc | 0.163 lb/in³ | |
Mechanical Properties |
|
| Hardness, Brinell | 200 | 200 | |
| Tensile Strength, Ultimate | 585 MPa | 84800 psi | |
| Tensile Strength, Yield | 450 MPa | 65300 psi | 0.2% YS |
| Elongation at Break | 25 % | 25 % | |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. MatWeb data and tools provided by MatWeb, LLC.
|