Allegheny Ludlum Titanium 6Al-4V ELI (UNS R56401)
Subcategory: Alpha/Beta Titanium Alloy; Metal; Nonferrous Metal; Titanium Alloy
Key Words: Ti 6-4; Titanium 6-4; ASTM B-265; ASTM F-136; ASME SB-265; AMS 4907-4; MIL-T-9046
| Component | Wt. % |  | | | Al | Max 6.5 | | | C | Max 0.08 | | | Fe | Max 0.25 | | | H | Max 0.015 | | | N | Max 0.03 | | | O | Max 0.13 | | | Ti | 90 | | | V | 4 | |
|
Material Notes: Titanium content above calculated as remainder. The ELI grade has lower impurity limits than standard titanium 6-4. Uses: applications requiring excellent fracture toughness and fatigue strength, aircraft, structural components, biomedical. Mechanical property data below is typical of annealed samples at room temperature. Information provided by Allegheny Ludlum.
| Physical Properties | Metric | English | Comments |
|
| Density | 4.43 g/cc | 0.16 lb/in³ | |
Mechanical Properties |
|
| Hardness, Rockwell C | 30 | 30 | |
| Tensile Strength, Ultimate | 828 MPa | 120000 psi | |
| Tensile Strength, Yield | 759 MPa | 110000 psi | 0.2% YS |
| Elongation at Break | 10 % | 10 % | |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. MatWeb data and tools provided by MatWeb, LLC.
|