MetalTek WASPALOY® Centri-Vac Nickel Cobalt Based Alloy
Subcategory: Metal; Nickel Base; Superalloy
Close Analogs: Wrought UNS N07001; Wrought Grade WASPALOY®
| Component | Wt. % |  | | | Al | 1.2 - 1.5 | | | C | 0.03 - 0.1 | | | Co | 12 - 15 | | | Cr | 18 - 21 | | | Mo | 3.5 - 4 | | | Ni | 55.15 - 62.52 | | | Ti | 2.75 - 3.25 | |
|
Material Notes:
Information provided by MetalTek
We're sorry, but our sources do not report any other information for this material. Sometimes you will see this message during a MatWeb internal update, especially around 07:00 GMT.
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. MatWeb data and tools provided by MatWeb, LLC.
|