AISI Type 310S Stainless Steel
Subcategory: Ferrous Metal; Metal; Stainless Steel; T 300 Series Stainless Steel
| Component | Wt. % |  | | | C | Max 0.08 | | | Cr | 24 - 26 | | | Fe | 54 | | | Mn | Max 2 | | | Ni | 19 - 22 | | | P | Max 0.045 | | | S | Max 0.03 | | | Si | Max 1.5 | |
|
Material Notes: Iron content above calculated as remainder. Low-carbon Type 310 - for welding. Information provided by Chevron-Phillips Chemical Company, LLC.
| Physical Properties | Metric | English | Comments |
|
| Density | 8 g/cc | 0.289 lb/in³ | (for Stainless 310) |
Mechanical Properties |
|
| Modulus of Elasticity | 200 GPa | 29000 ksi | (for Stainless 310) |
Thermal Properties |
|
| Specific Heat Capacity | 0.5 J/g-°C | 0.12 BTU/lb-°F | (for Stainless 310) |
| Thermal Conductivity | 14.2 W/m-K | 98.5 BTU-in/hr-ft²-°F | (for Stainless 310) |
| Melting Point | 1400 - 1455 °C | 2550 - 2650 °F | (for Stainless 310) |
| Solidus | 1400 °C | 2550 °F | (for Stainless 310) |
| Liquidus | 1455 °C | 2650 °F | (for Stainless 310) |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. MatWeb data and tools provided by MatWeb, LLC.
|