AISI Type 321 Stainless Steel, annealed bar
Subcategory: Ferrous Metal; Metal; Stainless Steel; T 300 Series Stainless Steel
| Component | Wt. % |  | | | C | 0.08 | | | Cr | 17 | | | Fe | 69 | |
| | Component | Wt. % |  | | | Mn | 2 | | | Ni | 11 | | | P | 0.045 | |
| | Component | Wt. % |  | | | S | 0.03 | | | Si | 1 | | | Ti | 0.15 | |
|
Material Notes: Similar to Type 304 except Ti content helps prevent chromium carbide precipitation resulting from welding or elevated temperatures. Stabilized at annealing temperatures between 950-1010°C (1750-1850°F). Resists scaling and vibration fatigue. Applications include aircraft exhaust stacks and manifolds, chemical processing equipment, weld equipment, jet engine parts.
| Physical Properties | Metric | English | Comments |
|
| Density | 8 g/cc | 0.289 lb/in³ | |
Mechanical Properties |
|
| Hardness, Brinell | 150 | 150 | |
| Hardness, Knoop | 170 | 170 | Converted from Brinell hardness. |
| Hardness, Rockwell B | 80 | 80 | |
| Hardness, Vickers | 157 | 157 | Converted from Brinell hardness. |
| Tensile Strength, Ultimate | 585 MPa | 84800 psi | |
| Tensile Strength, Yield | 240 MPa | 34800 psi | |
| Elongation at Break | 55 % | 55 % | in 50 mm |
| Modulus of Elasticity | 193 - 200 GPa | 28000 - 29000 ksi | |
| Charpy Impact | 165 J | 122 ft-lb | V-notch |
| Izod Impact | 135 J | 99.6 ft-lb | |
Electrical Properties |
|
| Electrical Resistivity | 7.2e-005 ohm-cm | 7.2e-005 ohm-cm | at 20ºC |
| Magnetic Permeability | 1.008 | 1.008 | at RT |
Thermal Properties |
|
| CTE, linear 20°C | 16.7 µm/m-°C | 9.28 µin/in-°F | 0 - 100ºC |
| CTE, linear 250°C | 17.1 µm/m-°C | 9.5 µin/in-°F | at 0-315°C (32-600°F) |
| CTE, linear 500°C | 18.5 µm/m-°C | 10.3 µin/in-°F | 0 - 540ºC |
| CTE, linear 1000°C | 20.5 µm/m-°C | 11.4 µin/in-°F | 20 - 925ºC |
| Specific Heat Capacity | 0.5 J/g-°C | 0.12 BTU/lb-°F | from 0-100°C (32-212°F) |
| Thermal Conductivity at Elevated Temperature | 16.1 W/m-K | 112 BTU-in/hr-ft²-°F | 100ºC |
| Melting Point | 1400 - 1425 °C | 2550 - 2600 °F | |
| Solidus | 1400 °C | 2550 °F | |
| Liquidus | 1425 °C | 2600 °F | |
| Maximum Service Temperature, Air | 870 °C | 1600 °F | Intermittent Service |
| Maximum Service Temperature, Air | 925 °C | 1700 °F | Continuous Service |
References for this datasheet.
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. MatWeb data and tools provided by MatWeb, LLC.
|