AISI Type 651 (19-9) Stainless Steel annealed at 980°C (1800°F), 88 HRB hardness, tested at 150°C (300°F)
Subcategory: Ferrous Metal; Heat Resisting; Metal; Stainless Steel; T 600 Series Stainless Steel
Key Words: UNS K63198, AMS 5369, AMS 5526, AMS 5527, AMS 5720, AMS 5721, AMS 5722, ASTM A453, ASTM A457, ASTM 458, ASTM A477, SAE J467(19-9 DL), MIL SPEC MIL-S-46042
| Component | Wt. % |  | | | C | 0.28 - 0.35 | | | Cr | 18 - 21 | | | Cu | Max 0.5 | | | Fe | 64 | | | Mn | 0.75 - 1.5 | |
| | Component | Wt. % |  | | | Mo | 1 - 1.75 | | | Nb | 0.25 - 0.6 | | | Ni | 8 - 11 | | | P | Max 0.04 | |
| | Component | Wt. % |  | | | S | Max 0.03 | | | Si | 0.3 - 0.8 | | | Ti | 0.1 - 0.35 | | | W | 1 - 1.75 | |
|
Material Notes: 0.89-1.33 mm thick sheet
| Physical Properties | Metric | English | Comments |
|
| Density | 7.94 g/cc | 0.287 lb/in³ | Room Temp. |
Mechanical Properties |
|
| Tensile Strength, Ultimate | 600 MPa | 87000 psi | |
| Tensile Strength, Yield | 317 MPa | 46000 psi | at 0.2% offset |
| Elongation at Break | 30 % | 30 % | in 50 mm |
| Machinability | 45 % | 45 % | Based on 100% machinability for AISI 1212 steel. |
Thermal Properties |
|
| CTE, linear 20°C | 15.3 µm/m-°C | 8.5 µin/in-°F | at 21-93°C (70-200°F), 16.3 µm/m°C at 21-205°C (70-400°F) |
| CTE, linear 250°C | 16.7 µm/m-°C | 9.28 µin/in-°F | at 21-315°C (70-600°F), 17.3 µm/m°C at 21-425°C (70-800°F) |
| CTE, linear 500°C | 17.6 µm/m-°C | 9.78 µin/in-°F | at 21-540°C (70-1000°F), 18.0 µm/m°C at 21-815°C (70-1500°F) |
| Specific Heat Capacity | 0.42 J/g-°C | 0.1 BTU/lb-°F | from 0-100°C (32-212°F) |
| Thermal Conductivity | 13.5 W/m-K | 93.7 BTU-in/hr-ft²-°F | at 21°C, 18.5 W/m-K at 425°C, 21.3 W/m-K at 650°C |
| Melting Point | 1420 - 1435 °C | 2590 - 2620 °F | |
| Solidus | 1420 °C | 2590 °F | |
| Liquidus | 1435 °C | 2620 °F | |
| Maximum Service Temperature, Air | 780 °C | 1440 °F | Continuous Service |
| Maximum Service Temperature, Air | 955 °C | 1750 °F | Intermittent Service |
References for this datasheet.
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. MatWeb data and tools provided by MatWeb, LLC.
|