Nickelvac® L-605 Nickel Superalloy, Heat Treatment: 1204°C (2200°F) Anneal
Subcategory: Cobalt Base; Metal; Nickel Base; Superalloy
Key Words: Allvac, an Allegheny Teledyne Company, UNS R30605; AMS 5759. ASTM F 90
| Component | Wt. % |  | | | C | 0.1 | | | Co | 53 | | | Cr | 20 | | | Fe | 0.5 | | | Mn | 1.7 | | | Ni | 10 | | | W | 15 | |
|
Material Notes: Nickel content calculated as remainder. Data provided by Allvac. Applications: High temperature applications, jet engine components, devices in high fatigue service.
| Physical Properties | Metric | English | Comments |
|
| Density | 9.22 g/cc | 0.333 lb/in³ | |
Mechanical Properties |
|
| Hardness, Rockwell B | 80 | 80 | |
| Tensile Strength, Ultimate | 1035 MPa | 150000 psi | |
| Tensile Strength, Yield | 414 MPa | 60000 psi | 0.2% Offset |
| Elongation at Break | 60 % | 60 % | |
| Reduction of Area | 40 % | 40 % | |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. MatWeb data and tools provided by MatWeb, LLC.
|