Carpenter AerMet 100, 875°F Aged
Subcategory: Alloy Steel; Ferrous Metal; Metal; Tool Steel
Close Analogs: UNS K92580
| Component | Wt. % |  | | | C | 0.23 | | | Co | 13.4 | | | Cr | 3.1 | | | Fe | 70.97 | | | Mo | 1.2 | | | Ni | 11.1 | |
|
Material Notes: An alloy providing high hardness and strength combined with exceptional ductility and toughness. This alloy should be considered for aircraft and aerospace structural components requiring high strength, high fracture toughness and exceptional stress corrosion cracking resistance. AerMet 100 may be considered for use up to about 800°F (427°C). This alloy is not subject to the same restrictions as AF1410, thus may be considered a substitute.
| Physical Properties | Metric | English | Comments |
|
| Density | 7.89 g/cc | 0.285 lb/in³ | |
Mechanical Properties |
|
| Tensile Yield Strength | 1780 MPa | 258000 psi | |
| Elongation at Break | 14.2 % | 14.2 % | |
| Reduction of Area | 63.8 % | 63.8 % | |
| Fatigue Strength | 945 MPa | 137000 psi | 10^7 cycles, R=-1, Kt=1 |
| Fracture Toughness | 108.454 MPa-m½ | 98.7 ksi-in½ | |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. MatWeb data and tools provided by MatWeb, LLC.
|