Allegheny Ludlum AL 418™ (Greek Ascoloy) Special Martensitic Stainless Steel
Subcategory: Ferrous Metal; Metal; Stainless Steel; T 400 Series Stainless Steel
Key Words: AMS 5508
| Component | Wt. % |  | | | Cr | 13 | | | Fe | 82 | | | Ni | 2 | | | W | 3 | |
|
Material Notes: Iron content above calculated as remainder. Uses incluse engine braces, turbine exhaust components, exhaust struts, stiffeners, and ducts. Information provided by Allegheny Ludlum
| Physical Properties | Metric | English | Comments |
|
| Density | 7.87 g/cc | 0.284 lb/in³ | |
Mechanical Properties |
|
| Hardness, Rockwell C | 25 | 25 | |
| Tensile Strength, Ultimate | 895 MPa | 130000 psi | |
| Tensile Strength, Yield | 725 MPa | 105000 psi | 0.2% YS |
| Elongation at Break | 15 % | 15 % | |
Some of the values displayed above may have been converted from their original units and/or rounded in
order to display the information in a consistant format. Users requiring more precise data for scientific or
engineering calculations can click on the property value to see the original value as well as raw conversions
to equivalent units. We advise that you only use the original value or one of its raw conversions in your
calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use
regarding this information. MatWeb data and tools provided by MatWeb, LLC.
|